Weld Mold 959 .035 H-13 Tig Welding Filler Rod 1lb, Blacksmith Power Hammer Dies For Sale


Weld Mold 959 .035 H-13 Tig Welding Filler Rod 1lb, Blacksmith Power Hammer Dies
When you click on links to various merchants on this site and make a purchase, this can result in this site earning a commission. Affiliate programs and affiliations include, but are not limited to, the eBay Partner Network.



Buy Now

Weld Mold 959 .035 H-13 Tig Welding Filler Rod 1lb, Blacksmith Power Hammer Dies:
$29.99

Weld Mold 959.035 H-13 Tig Welding Filler Rod 1lb, Blacksmith Power Hammer Dies

GREAT ON FORGING AND HAMMERDIES FOR THE BLACKSMITH BLADESMITH AND KNIFE MAKER.

H-13 is Hot Work Tool Steel

From the Weld Mold site:

Weld Mold 959 produces hot working weld deposits that are tungsten-free, homogeneous, porous-free, dense, and may be annealed and rehardened, if necessary. Matches A.I.S.I. H-13 tool steel heat treatment.

Primarily designed for use on tools and dies subject to heat checking and wear. Examples include: die casting dies used in the aluminum, magnesium, and zinc die casting industries as well as for repair of press forging dies and inserts. May be used on other hot or cold working units such as shears, punches, trim sections, etc

For repairs, prepare area to be welded by removing all cracks, heat checks or other defects. Clean area of any slag, scale, rust or drawing compounds. Preheat die blocks and other units where the entire working surface is to be welded to 800º F. On other alloys preheat and post-heat according to the base metal. Maintain temperature during welding. Use the stringer bead technique. Peen the weld when forgeable to relieve stresses. After welding, cool in still air to 300º F to obtain the ultimate grain refinement and uniform hardness in the weld deposit. Temper at 1000º F for one hour per inch of thickness. Cool in still air to room temperature

Please e-mail with any questions

Winner must make contact including payment arrangements within 3 days of sale end, payment must be received within 10 days of sale end. I reserve the right to resell any item if I have not received contact from the winner within 3 days, and or received payment for any item within 10 days of the sale end. I accept PayPal. I try to descibe exactly what the item is. Please email any questions. All sales final. I do participate in leaving response on . Thanks for looking and good luck!



.

.